Technique of Strength Increasing of Working Pipeline Parts with the Help of Well-Bond Goints

Григорій Семенович Тимчик, Олександр Олександрович Подолян

Abstract


Background. Getting high efficiency of enhancing pipeline of small and medium diameter using well-bond joints is complicated, because of the low modulus of elasticity compounds used to form the under-join layer.

Objective. Development of the strength increasing technique of the high pressure pipelines parts using the well-bond joints is the aim of this study.

Methods. Strength increasing technique of a working pipeline with the help of well-bond joints was used.

Results. The strength increasing technique of the high pressure pipelines parts using the well-bond joints, which are filled with molten metal with a high modulus of elasticity, is offered. The operations of forming the under-joint layer with parameters providing achievement of maximum tension decrease level in strengthened pipe providing and equal load distribution between a side of a pipe part under repair and joint covering are considered.

Conclusions. The offered technique gives an opportunity to increase efficiency of strengthening the medium and small pipes diameter pipes.

Keywords


Coupling; Nondestructive control; Diagnostics; Repair; Gas passage line; Pipeline; Pressure

References


M.V. Bekker et al., Repair of Gas-Main Pipelines under Pressure. Kyiv, Ukraine: Kyi, 2008, 240 p. (in Ukrainian).

Gas-Main Pipelines, Arc Welding Repair in Operating Conditions, GBN V.3.1-00013741-12:2011, Ministry of Energetics and Coal Industry ofUkraine, Kyiv, 2011 (in Ukrainian).

G.S. Tymchik and A.A. Podolian, “The quality control system installation glued-welded joint on the trunk gas pipeline under the high pressure”, Naukovi Visti NTUU “KPI”, no. 6, pp. 138–144, 2012 (in Russian).

Technological Instruction for Gas-Main Pipelines under Pressure with the Use of Arc Welding, DK “Ukrtransgas”,Kyiv,Ukraine, 2000, 96 p. (in Ukrainian).

I.V. Oryniak et al., “Method for repair of operating pipeline by means of couplings with inner filling”, UA Patent 98440, May 10, 2012 (in Ukrainian).

Composites Handbook, Dzh. Liubin, Ed. Moscow, Russia: Mashinostroenie, 1988, book 1, 448 p., book 2, 584 p. (in Russian).

A.A. Podolian et al., “Method for reinforcement of a pipeline by means of couplings with inner filling with control of quality of works (variants)”, UA Patent 98601, May 25, 2012 (in Ukrainian).

G.S. Tymchik and A.A. Podolian, “Techonlogy of ultrasonic control of the well-bonded pipe coupling space filling”, Naukovi Visti NTUU “KPI”, no. 2, pp. 103–109, 2014 (in Russian).


GOST Style Citations


  1. Ремонт магістральних трубопроводів під тиском / М.В. Беккер, В.С. Бут, Р.М. Говдяк и др. – К.: Кий, 2008. – 240 с.

  2. Магістральні газопроводи, ремонт дуговим зварюванням в умовах експлуатації: ГБН В.3.1-00013741-12:2011. – К.: Міністерство енергетики та вугільної промисловості України, 2011. – 152 с.

  3. Тымчик Г.С., Подолян А.А. Система контроля качества монтажа клеесварной муфты на магистральном газопроводе высокого давления газопроводов // Наукові вісті НТУУ “КПІ”. – 2012. – № 6. – С. 138–144.

  4. Технологічна інструкція з ремонту магістральних газопроводів під тиском з застосуванням дугового зварювання. – К.: ДК “Укртрансгаз”, 2000. – 96 с.

  5. Спосіб ремонту діючого трубопроводу за допомогою муфт з внутрішнім заповненням: Пат. 98440 України, МПК (2006) F16L 55/175 / І.В. Ориняк, О.О. Подолян, С.В. Пудрий та ін. – Заявлено 01.03.2012; Опубл. 10.05.2012, Бюл. № 18.

  6. Справочник по композиционным материалам: В 2-х кн. / Под ред. Дж. Любина. – М.: Машиностроение, 1988. – Кн. 1. – 448 с.; Кн. 2. – 584 с.

  7. Спосіб муфтового ремонту трубопроводу: Пат. 98601 України, МПК (2006) F16L 55/175 / О.О. Подолян, С.В. Пудрий, О.І. Томашук та ін. – Заявлено 30.03.2012; Опубл. 25.05.2012, Бюл. № 18.

  8. Тымчик Г.С., Подолян А.А. Технология ультразвукового контроля заполнения подмуфтового пространства клеесварной муфты трубопроводов // Наукові вісті НТУУ “КПІ”. – 2014. – № 2. – С. 103–109.




DOI: http://dx.doi.org/10.20535/1810-0546.2015.2.91531

Refbacks

  • There are currently no refbacks.